MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Inno-Comp INNOBATCH® PPH 3160 60% Talc Filled Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: INNOBATCH® PPH 3160 is a 60% talc-filled polypropylene homopolymer based masterbatch. This grade is available in natural colored form.

These products that are offered under the brand name INNOBATCH® are recommended for the area of packaging materials, but they can be used for manufacturing household appliances and outdoor furniture and for other purposes as well. The raw material having filler content is a semi-finished product from a user point of view; this allows the user to determine the optimal feeding rate during the processing operation.

Information provided by INNO-COMP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 53 - 63 %
@Temperature 600 °C
53 - 63 %
@Temperature 1110 °F
ISO 3451-1/A
Storage Temperature <= 60.0 °C<= 140 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.070 %<= 0.070 %
 
Descriptive Properties
Resin DesignationPP-H TD60ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Inno-Comp INNOBATCH® PPH 6160 60% Talc-Filled Polypropylene Homopolymer
Inno-Comp INNOBATCH® PPH 6160 60% Talc Filled Polypropylene Homopolymer
A.D. Compound Adene NTWA Homopolymer 60% Talc Filled Polypropylene

PINNO911 / 150111

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.