MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Aremco’s refractory coatings offer the ultimate protection of high temperature components used in the processing of ceramics, glass, metals, and plastics.

Features

  • Ultra Hi-Temp Resistance
  • Non-Wetted by Molten Metals, Salts, Glass & Plastics
  • High Lubricity for Easy Part Release
  • Minimizes Cast Surface Defects
  • Increases Mold & Die Life
  • For Use in Oxidizing, Reducing & Vacuum Atmospheres
Applications:
  • Composite Forming
  • Glass Forming
  • Metal Casting
  • Injection Molding
  • Ceramic Hot-Pressing
  • Metal Powder Sintering
  • Welding
  • Brazing
Product Highlights: This high purity alumina, two-part coating seals alumina fiberboards and shapes to fill porosity and resist molten metals to 3200°F (1760°C). Increases heat reflectivity to improve furnace efficiency by reducing ramp up times.

Key Words: Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.46 g/cc
Density 12.0 lb/gal
Solids Content 56 %volume
 81.3 %weight
pH 4.0 - 5.0Coating pH
Viscosity 100 - 200 cP
Thickness 1.00 milDry Film Thickness
 1.80 milWet Film Thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 3200 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Cure Time 2.00 hour
@Temperature 93.3 °C
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
 
Descriptive Properties
ColorWhite
Coverage ft2/gal899Theoretical Coverage at 1 mil dry film thickness
Mix Ratio75:25Powder:Liquid
Thinner634AL-T
Weight/Gallon12 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material
Morgan Advanced Ceramics Engineered Fibers Refractory Ceramic Fiber Bulks Thermal Ceramic
Mid-Mountain Materials THERMOSEAL® P110 Thermal Coating
MarkeTech Carbon Nanofoam

CAREM58 / 599

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.