Appearance: Silver Cure: Heat cure Product Benefits: - Electrically conductive
- Stencil or screen printable
- Pb-free alternative to solder
- Controlled particle size
- Low cure temperature
Application: Electrically Conductive Adhesive Filler Type: Silver Surfaces Sn, Sn/Pb and OSP coated Cu Typical Package Application: SMD component attach LOCTITE ABLESTIK CE 3104WXL is an electrically conductive epoxy adhesive that is a Pb-free alternative to solder. This product uses a unique blend of fillers with tightly controlled particle sizes to provide ultra-fine pitch resolution (<500µm) when printed using either a stainless steel mesh screen or a metal mask stencil. The lower surface tension versus solder means no bridging on fine-pitch assembly patterns. Information provided by Loctite® |