MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chi Mei Wonderlite® PC-115P PC Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: Complies with Bio-compatibility test (ISO 10993-4,5,10,11). Gamma resistance (particular color). Applications: Medical

WONDERLITE® is a polycarbonate (PC) resin polymerized using the double hydroxy compounds of bisphenol-A (BPA) and the carbonate compounds of diphenyl carbonate (DPC), produced via our unique transesterification (melting) method. This resin offers glass-like transparency, high heat resistance, ultra high impact resistance, and dimensional stability, making it suitable for a wide range of applications.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cmISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
Melt Volume Rate (ml/10 min.); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa50mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527
Elongation at Break 120 %50mm/min; ISO 527
Flexural Strength 90.0 MPa2mm/min; ISO 178
Flexural Modulus 2.40 GPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 70.0 kJ/m²
@Thickness 3.17 mm
ISO 180/1A
Charpy Impact, Notched 70.0 kJ/m²1/8"; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 80.0 µm/m-°CISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 128 °CUnannealed; ISO 75/A
 143 °CAnnealed; ISO 75/A
Vicat Softening Point 145 °C
@Load 5.00 kg
50°C/hr; ISO 306
 150 °C
@Load 1.00 kg
50°C/hr; ISO 306
Flammability, UL94 V-2
@Thickness 2.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHI9952 / 280849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.