MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm ACRYLITE® Edgelight 8N LD96 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Edgelight 8N LD96 Acrylic Molding Compound is a highly transparent light guide material based on ACRYLITE® 8N. In addition to the typical properties of ACRYLITE®, such as
  • Excellent weather resistance
  • UV-stability
  • Good flow, high mechanical strength
ACRYLITE® Edgelight 8N LD96 is developed for edge lit LED applications. The light scattering properties convert the light guide to a full illuminated panel. Furthermore, the material allows for a completely transparent view through the light guide when it is not illuminated. This opens a new degree of freedom for designers. ACRYLITE® Edgelight 8N LD96 is recommended for panels with a distance of 48 cm to 96 cm between two light injecting LED strips.

Application: Injection molding or extrusion.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 1183
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Water Absorption <= 0.30 %<= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 3.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.3 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength 80.0 MPa11600 psiASTM D638
Elongation at Break 4.0 - 6.0 %4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %4.0 - 6.0 %ASTM D638
Tensile Modulus 3.20 GPa464 ksiASTM D638
Flexural Strength 128.9 MPa18700 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Izod Impact, Notched 0.190 J/cm
@Thickness 6.35 mm
0.356 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
40.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.35 mm
212 °F
@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 108 °C
@Load 5.10 kg
226 °F
@Load 11.2 lb
50°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %ASTM E313
Transmission, Visible >= 92 %>= 92 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 252 °C464 - 486 °F
Mold Temperature 38.0 - 80.0 °C100 - 176 °FInjection Molding
Drying Temperature 80.0 °C176 °FPredrying
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourPredrying, Desiccant-Type Drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9341 / 319958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.