MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt NORSODYNE® Y 93172 Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Tetrahydrophthalic

Appearance: Amber - Light - Transparent

Main resin characteristics: Very long shelf life, Preaccelerated

Main applications: Mastics, Putties

Curing cycle: 16 h at 40°C (+ 2 h at 120°C for HDT)

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Solids Content 64 - 68 %64 - 68 %MT-CU001C
Brookfield Viscosity 450 - 550 cP450 - 550 cPsp 2 rpm 50; MT-CUT23V
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.6 MPa3280 psiISO 527
Elongation at Break 34.46 %34.46 %ISO 527
Tensile Modulus 1.235 GPa179.1 ksiISO 527
Flexural Strength 83.0 MPa12000 psiISO 178
Flexural Modulus 2.615 GPa379.3 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Cure Time 0.200 - 0.300 min
@Temperature 23.0 °C
0.00333 - 0.00500 hour
@Temperature 73.4 °F
Peak, Reactivity at 23°C + 2% PBO50; MT-CU162R
Gel Time 7.00 - 9.00 min
@Temperature 23.0 °C
7.00 - 9.00 min
@Temperature 73.4 °F
Reactivity at 23°C + 2% PBO50; MT-CU162R
Shelf Life 9.00 Month9.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm130 - 150°CMT-CU162R; Reactivity at 23°C + 2% PBO50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9374 / 231969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.