MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT ALPA-SIL 18101 Silicone Molding Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: Notch-resistant, condensation crosslinking silicone filling compound particularly for casting polyester resin.

Key Features

  • Good flowing behavior
  • Very good elastic properties
  • Outstanding stability to polyester resins
  • Suitable for block moulds and skin moulds with strong undercuts
Application: casting polyester resin, printing pads, block moulds and skin moulds with strong undercuts

Cured Product: Standard climate DIN 50 014 - 23/50-2. Vulcanizate tested after 7 days at room temperature

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³B; DIN 53 479
 1.09 g/cc0.0394 lb/in³A; DIN 53 479
Brookfield Viscosity 20 cP20 cPB
 29000 cP29000 cPMixed
 30000 cP30000 cPA
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
Storage Temperature 5.00 - 30.0 °C41.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1818DIN 53 504, S 3 A
Tensile Strength 3.00 MPa435 psiDIN 53 504, S 3 A
Tear Strength 17.2 kN/m98.0 pliASTM D 624, Die B
 
Processing PropertiesMetricEnglishComments
Cure Time 1080 min18.0 hourDe-mould Time / Full Cure
Pot Life 100 min100 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
AppearanceTranslucent
ColorTranslucentA
 TransparentCured Product
Cure typeCondensation
Mix Ratio100:3By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL082 / 314565

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.