MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SSAB Tunnplat Domex® Wear Steel Sheet
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Domex® Wear is a new grade of steel sheet in the Domex® range, and its main distinguishing features are good wear resistance, high strength, good bendability, high toughness and good weldability. The wear resistance of Domex® Wear is close to that of much harder quenching and tempering steels.

Uses: For components subjected to moderate abrasive wear caused by hard particles, such as stones, sand, ore or slurries. In the building industry: concrete mixers, hoppers. In the transport industry: truck platforms, tippers, sludge conveyors, refuse collection trucks. In agriculture: plough shares, seed conveyors. In the mining industry: fans, screws conveyors.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccEstimated by MatWeb
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 265
Tensile Strength, Ultimate >= 800 MPa
Tensile Strength, Yield 780 MPa
Elongation at Break 15 %A5
Impact 34J/cm²; -20°C; longitudinal
Bend Radius, Minimum >= 2.0 t
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.040 %
Carbon, C 0.17 %
Chromium, Cr 0.30 %
Iron, Fe 97.14 %As Remainder
Manganese, Mn 1.8 %
Molybdenum, Mo 0.10 %
Phosphorus, P 0.010 %
Silicon, Si 0.30 %
Sulfur, S <= 0.010 %
Titanium, Ti 0.14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® 1200 DP High-strength Steel
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate
SSAB Tunnplat Domex® 500MC HSLA Steel
SSAB Tunnplat Domex® 700MC HSLA Steel
SSAB Tunnplat Domex® 740XP Extra High-strength Cold-forming Steel

NTUNN93 / 19585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.