MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Marco Polo MarPol LDC 710 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: MARPOL® LDC 710 is a high speed, lightweight-coating resin for use with paper, films and other base stocks. This resin can be extrusion coated at line speeds of 1,200 ft/min. or higher. Applied to paper, foil, cellophane, polyester film and other base stocks by conventional extrusion coating processes. The maximum recommended melt temperature is 625°F (330 °C).

Recommended application: Flexible packaging, milk cartons, industrial papers, foil mounting, single-ply bags, pouch bags, board trays, fiber drums, corrugated boxes and fiberboard containers.

Additives: Antiblock - no, slip - no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D2240
Tensile Strength at Break 12.0 MPaASTM D638
Tensile Strength, Yield 13.0 MPaASTM D638
Elongation at Break 226 %ASTM D638
Flexural Modulus, 1% Secant 215 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °CASTM D3418
Vicat Softening Point 95.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO087 / 283684

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.