MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultraform® N2200 G43 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccISO 1183
Moisture Absorption at Equilibrium 0.15 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 0.90 %ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 2577
Melt Flow 6.622 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 164 MPa
@Load 36.5 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength at Break 115 MPa5 mm/min; ISO 527-2
Elongation at Break 3.0 %ISO 527-2
Modulus of Elasticity 7.30 GPaISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 5.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 7.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 4500 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 100 Hz
IEC 60250
 4.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 43.0 kV/mmIEC 60243-1
Dissipation Factor 0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
 600 VTest solution B; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
DIN 53752
Melting Point 170 °CDIN 53765
Maximum Service Temperature, Air 110 °C
Deflection Temperature at 1.8 MPa (264 psi) 161 °CISO 75-2
Vicat Softening Point 160 °CISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °CHopper Throat
Zone 1 205 °CFeed zone
Zone 2 205 °CCompression
Zone 3 210 °CMetering-zone
Zone 4 210 °CNozzle
Melt Temperature 190 - 230 °CInjection-molding
 210 °COptimal
Mold Temperature 60.0 - 120 °CInjection-molding
 100 °COptimal
Drying Temperature 100 °C
Dry Time 3 hour
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed<0.3 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® N2720 M63 30% Mineral Filled POM
BASF Ultraform® N 2200 G53 UNC Q600 25% Glass Filled POM
Celanese Hostaform® C9021 M Acetal Copolymer with Molybdenum Disulphide
KEP Kepital® FG2025K Acetal Copolymer, 10% Glass Fiber
304 Stainless Steel

PBASG0141 / 131774

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.