MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient PolyOne® 4763A Ethylene-Propylene Diene Elastomer (EPDM) Compound  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

PolyOne Chemical Cure EPDM wire and cable compounds include a full range of thermoset elastomers ranging from natural rubber to fluoroelastomers. Rubber offers excellent thermal and chemical resistance in a broad range of Durometer (Shore A and D) for applications in the wire and cable industry. PolyOne 4763A is a colorable candidate for UL multi-listing. When used in appropriate construction, this product will pass UL-44 for building wire and tray cable applications. Rated VW-1 for XHHW, RHH-RHW, USE, and SIS.

Description/Features:

  • VW-1
  • XHHW
  • RHH-RHW
  • USE
  • SIS

Market:

  • Wire & Cable

Note: Tensile Strength and Elongation measured on No. 14 AWG with 30mm Wall.
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1850 psiType 4 - Flexibles, Break, 20 in/min; ASTM D638
Elongation at Break 350 %Type 4 - Flexibles, 20 in/min; ASTM D638
Crush Resistance 595.01 kgUL1581
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
Glancing Impact Retention0.68UL 1581
Limited Score Retention26%UL 1581
Mechanical Water Absorption6.82724343219182E-05oz/in²7 days @ 82ºC, UL 1581
Oven Aged - Retention of Elongation (ROE)79%207ºF(97ºC), 2,160 hrs (90 days), 0.075 in, UL Standard
 84%250°F(121°C), 168 hrs (7 days), 0.075 in, UL Standard
Oven Aged - Retention of Tensile Strength (ROT)94%207ºF(97ºC), 2,160 hrs (90 days), 0.075 in, UL Standard
 95%250°F(121°C), 168 hrs (7 days), 0.075 in, UL Standard

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient PolyOne® ND-10 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Avient PolyOne® 4475 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Avient PolyOne® 4474 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Armacell Monarch® F-03092 (Black) EPDM Foam
Armacell Monarch® F-03091 (Black) Pure EPDM Foam

PH1PO3442 / 45079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.