MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 133 GH Nylon 66, 33% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass Fiber, 33% Filler by Weight

Additive: Heat Stabilizer; Lubricant

Features: Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated

Automotive Specifications: 3M 11-0003-5762-1; CHRYSLER MS-DB-41 CPN1900 Color: BK001 Black; CHRYSLER MS-DB-41 CPN2224 Color: Non-matched Color; FORD ESB-M4D133-A; FORD ESB-M4D89-A; FORD WSK-M4D663-A; GM GMP.PA66.013 Color: Natural; GM GMW3038P-PA66-GF35H

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccASTM D792
Water Absorption 0.90 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0015 - 0.0040 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25500 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Elongation at Yield 3.0 %ASTM D638
Flexural Strength 40000 psiASTM D790
Flexural Modulus 1.25e+6 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 410 V/mil
@Thickness 3.00 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µin/in-°FASTM D969
Deflection Temperature at 1.8 MPa (264 psi) 480 °FUnannealed; ASTM D648
UL RTI, Electrical 203 °F
@Thickness 0.762 mm
UL 746
 230 °F
@Thickness 1.52 mm
UL 746
 230 °F
@Thickness 3.05 mm
UL 746
UL RTI, Mechanical with Impact 203 °F
@Thickness 0.762 mm
UL 746
 230 °F
@Thickness 1.52 mm
UL 746
 230 °F
@Thickness 3.05 mm
UL 746
UL RTI, Mechanical without Impact 266 °F
@Thickness 0.762 mm
UL 746
 266 °F
@Thickness 1.52 mm
UL 746
 266 °F
@Thickness 3.05 mm
UL 746
Flammability, UL94 HB
@Thickness 0.762 mm
Oxygen Index 25 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 475 - 495 °F
Middle Barrel Temperature 505 - 525 °F
Front Barrel Temperature 515 - 540 °F
Nozzle Temperature 515 - 540 °F
Melt Temperature 495 °F
 505 - 540 °F
Mold Temperature 140 - 200 °F
Drying Temperature 175 °F
Injection Pressure 5000 - 20000 psi
Screw Speed 60 - 120 rpm
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0468 / 236959

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.