MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ebbtide Polymers 920 Transparent ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: The property values below are typical data under specific test conditions and are not intended for product design use.

Information provided by Ebbtide Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccFloat and Sink Method
Water Absorption 0.30 %24 hr immersion; ASTM D570
Viscosity 350000 - 500000 cP
@Temperature 220 °C
Plunger-type Viscometer
Melt Flow 19 - 23 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength at Break 37.0 MPaASTM D638
Tensile Strength, Yield 48.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Elongation at Yield 3.5 %ASTM D638
Flexural Yield Strength 77.0 MPaASTM D790
Flexural Modulus 2.30 GPaASTM D790
Izod Impact, Notched 0.900 J/cm
@Thickness 12.7 mm
ASTM D256
 1.00 J/cm
@Thickness 3.17 mm
ASTM D256
 0.600 J/cm
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 0.700 J/cm
@Thickness 3.17 mm,
Temperature 0.000 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °CUnannealed; ASTM D648
Flammability, UL94 HBAll Colors
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 85 %Transparent, but thickness unknown

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Absolac® 920 ABS
Chi Mei Polylac® PA-758 ABS - Transparent
INEOS Styrolution Absolan® 2300 SAN
Cotronics Resbond™ 920 High Temperature Ceramic Adhesive, Thermally Conductive
INEOS Styrolution Terluran® HI-12 ABS

PZ9EB35 / 21437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.