MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Maxxam™ 34-1520 Silver Metallic TFPP Polypropylene Homopolymer (PP Homopolymer)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Filler Content 20 %Talc Filler
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.7 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 20 %Type I, 51 mm/min; ASTM D638
Flexural Strength 51.7 MPaASTM D790
Flexural Modulus 2210 MPaASTM D790
Izod Impact, Notched 32.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 16.0 - 50.0 °C
 
Descriptive Properties
AppearanceSilver
FeaturesGeneral Purpose
 Homopolymer
FormsPellets
Generic MaterialPP Homopolymer
Generic NamePolypropylene Homopolymer (PP Homopolymer)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVALEN PQ 81 T 15 PP, 15% mineral filling
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin
Borealis Daplen™ EE255AE Polypropylene TPO Compound

PH0POL1004 / 145573

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.