MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAGON® B 1530 Colorant
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset

Material Notes: VESTAGON® B 1530 is a polyisocyanate adduct used in combination with hydroxyl functional resins. Due to the e-Caprolactam blocked NCO-groups it is stable during processing up to the unblocking temperature of more than 170°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.670 g/ccDIN 53 466
Density 1.14 g/ccDIN 53 479
 
Thermal PropertiesOriginal ValueComments
Melting Point 62.0 - 82.0 °CDIN 53 736
Glass Transition Temp, Tg 41.0 - 53.0 °CDSC
Flash Point 195 °CISO 2592
Ignition Temperature 440 °CDIN 51 794
 
Descriptive Properties
NCO content (% wt)<1DIN EN ISO 11 909; free
 14.8-15.7DIN EN ISO 11 909; total
NCO-equivalent (g/Eq)275

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAGON® B 1530 PUR System
Evonik VESTAGON® B 68 Colorant
Evonik VESTAGON® B 31 Colorant
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel

PHUMB380 / 81382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.