MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softening point.

Application: Pearlbond™ 125H can be used for making heat-sealable fabrics (thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 2781
Viscosity 890000 cP
@Temperature 160 °C
890000 cP
@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Melt Flow 35 - 55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
35 - 55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ISO 868
Tensile Strength at Break 18.0 MPa2610 psiISO 527
Elongation at Break 520 %520 %ISO 527
100% Modulus 4.00 MPa
@Strain 100 %
580 psi
@Strain 100 %
ISO 527
300% Modulus 7.00 MPa
@Strain 300 %
1020 psi
@Strain 300 %
ISO 527
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 - 140 °C266 - 284 °FMQSA 111
Softening Point 110 - 130 °C230 - 266 °FMQSA 70A
 
Processing PropertiesMetricEnglishComments
Zone 1 120 - 130 °C248 - 266 °F
Zone 2 130 - 140 °C266 - 284 °F
Zone 3 140 - 150 °C284 - 302 °F
Zone 4 145 - 155 °C293 - 311 °F
Die Temperature 145 - 155 °C293 - 311 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer

PMES14 / 52912

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.