MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bostik Durabond® D-733™ Acrylic Cove Base Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Description: DURABOND® D-733™ Acrylic Cove Base Adhesive is a high performance, medium set, acrylic adhesive. The wet suction of D-733 is strong enough to hold down corners on cove base.

Product Benefits:

  • Excellent wet suction
  • Easy trowel application
Performance Characteristics:
  • Fast grab
  • Holds corners
  • Good open time
Suggested Uses: D-733 Acrylic Cove Base Adhesive may be used for bonding vinyl and rubber cove base to: concrete, masonry, drywall, painted surfaces, wood, and particle board.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0528 lb/in³
Solids Content 72 %72 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 - 45.0 min0.500 - 0.750 hourSet Up Time
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Adhesive
Henkel Loctite® Durabond® E-20NS Epoxy Adhesive
Henkel Loctite® Durabond® E-20HP Epoxy Adhesive
Henkel Loctite® Durabond® E-120HP Epoxy Adhesive
Henkel Loctite® Durabond® E-05CL Epoxy Adhesive

PBOSTK023 / 191559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.