MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-115 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment

Agency Ratings: ISO 10993 Part 5

Processing Method: Extrusion; Injection Molding

Forms: Pellets

Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/ccASTM D792
Linear Mold Shrinkage 0.039 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.034 in/inASTM D955
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37ASTM D2240
Tensile Strength at Break 1080 psiASTM D412
Tensile Stress at Strain 125 psi
@Strain 100 %
ASTM D412
 220 psi
@Strain 200 %
ASTM D412
 320 psi
@Strain 300 %
ASTM D412
Elongation at Break 650 %ASTM D412
Tear Strength 21.0 kN/mASTM D624
Compression Set 13 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 315 °F
Middle Barrel Temperature 280 - 320 °F
Front Barrel Temperature 300 - 340 °F
Nozzle Temperature 340 - 380 °F
Zone 1 280 - 300 °F
Zone 2 300 - 320 °F
Zone 3 320 - 360 °F
Zone 5 340 - 380 °F
Die Temperature 360 - 400 °F
Melt Temperature 340 - 380 °FProcessing Temperature
Mold Temperature 70.0 - 100 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-727 ABS
Chi Mei Polylac® PA-709 ABS
Ineos L12Z-00 Polypropylene Impact Copolymer
RTP Company RTP 2720 S-30A Saturated Styrenic Block Copolymer
Teknor Apex Medalist® MD-110 Thermoplastic Elastomer

PTEKNO700 / 128878

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.