MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
ALM TPE-210-S Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Elastomer, TPE

Material Notes:
  • A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and abrasion resistance.
  • TPE 210-S processes at a much lower temperature (~ 80 C) when compared to other commercially available flexible materials.
  • TPE 210-S is 100% recyclable

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.370 g/ccASTM D1895
Density 1.03 g/ccSintered; ASTM D792
Particle Size 20 - 130 µmD10-D90
 85 µmD50
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 235 °C
3 min; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 110 %uninfiltrated; ASTM D638
Tensile Modulus 8.00 MPaASTM D638
Flexural Modulus 3.00 MPa
@Temperature 100 °C
ASTM D790
 13.0 MPa
@Temperature 23.0 °C
ASTM D790
 23.0 MPa
@Temperature -40.0 °C
ASTM D790
Tear Strength 5.00 kN/m
@Temperature 100 °C
Initial, Die C; ASTM D624
 6.00 kN/m
@Temperature 23.0 °C
Initial, Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 353H-18 Wheel; ASTM D4060
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+13 ohm-cmASTM D257
Surface Resistance 1.90e+13 ohmASTM D257
Dielectric Constant 2.9
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °CASTM D3418
 
Descriptive Properties
Shore Hardness (scale not noted)40uninfiltrated, ASTM D2240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems
ALM PA 250 Nylon 12 SLS Prototyping Polymer
ALM FR 106 Nylon 11 SLS Prototyping Polymer
ALM D80-ST Nylon 11 SLS Prototyping Polymer
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer

PALP80 / 177151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.