MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Vistalon™ 404 Ethylene Propylene Copolymer Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Description: Vistalon 404 rubber is a low Mooney, low ethylene copolymer with a broad molecular weight distribution. It is applicable for use in formulations for molded and mechanical goods. This product is sold in dense bales.

Key Features: Easy processing and mixing.

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 28
@Temperature 125 °C
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
 
Descriptive Properties
Ethylene Content45.0 wt%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui NOTIO™ PN-2070 Nano-crystal Structure Controlled Elastomer
ExxonMobil Vistalon™ 1703P EPDM
ExxonMobil PP7033L1 Polypropylene Impact Copolymer
ExxonMobil Vistalon™ 3702 Ethylene Propylene Diene Terpolymer Rubber
ExxonMobil Vistalon™ 706 Ethylene Propylene Copolymer Rubber

PEXA929 / 125972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.