MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® L 25 W 20 X PA12-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. The main features of Grilamid L 25 W 20 X are:
  • Exceptional impact strength even at low temperatures
  • Semi-flexible
  • UV and heat stability
  • Good chemical resistance
  • Low density, low weight
  • Very easy to process
Application examples: Grilamid L 25 W 20 X is particularly suitable for the production of semi-flexible tubes and profiles requiring good low temperature impact strength for both automotive an industrial applications.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccDry; ISO 1183
Water Absorption 1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
@Time 15.0 sec
Conditioned; ISO 868
Tensile Strength at Break 35.0 MPaConditioned; ISO 527-1/-2
 40.0 MPaDry; ISO 527-1/-2
Tensile Strength, Yield 30.0 MPaDry; ISO 527-1/-2
 30.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 20 %Dry; ISO 527-1/-2
 20 %Conditioned; ISO 527-1/-2
Tensile Modulus 450 MPaDry; ISO 527-1/-2
 450 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 140 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°CISO 11359-1/-2
Melting Point 174 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AdditivesPlasticizer
AutomotiveCompressed air systems
 Fuel systems
 Hydraulic systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
Product AttributesFlexible
 High viscosity
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 2D 25 W 20 X nat PA612-I
EMS-Grivory Grilamid® 2D 25 W 20 X black PA612-I
EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 43)
EMS-Grivory Grilamid® 2S 25 W 20 X nat PA610-I

PGRH048 / 156757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.