MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

HB Fuller Swift®melt 82674 Hot Melt Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 82674 is specifically formulated as a light colored adhesive to form permanent bonds which uniquely combines high peel strength with low viscosity, enabling it to be applied with spray as well as conventional application equipment. 82674 is recommended for general purpose applications where ease of coating and high performance is desired. Typical applications include peel and stick flooring.

Features and Benefits:

  • Low viscosity allowing wider application temperature and more effective machining
  • Very high peel strength and high heat resistance
  • Excellent quick tack
  • Broad application methods including spray, extrusion, and slot die
  • Good adhesion to a variety of substrates and film stocks
  • Good peel, shear and tack properties

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 4900 - 7400 cP
@Temperature 149 - 177 °C
4900 - 7400 cP
@Temperature 300 - 350 °F
Storage Temperature -6.67 - 48.9 °C20.0 - 120 °F
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 1.49 kN/m8.50 pli
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Softening Point 111 °C232 °FMettler
Minimum Service Temperature, Air 149 °C300 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorLight Yellow
ConsistencyViscous LiquidSolid at Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL168 / 316959

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.