MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ALM TPE 410 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: TPE 410 is designed for a variety of different applications which require a strong durable yet flexible material. It’s ideal for short series production work for elastic parts that will see a variety of applications.

Highlights:

  • High impact resistance at lower temperatures
  • Excellent processability without the requirement of pretreatment
  • Material is soft to the touch
  • Low energy loss in a wide variety of temperature ranges
Applications:
  • Footwear
  • Sports equipment including hockey and football helmets
  • Seating applications
  • Automotive

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/ccASTM D1895
Density 0.700 - 0.960 g/ccSintered; ASTM D792
Particle Size 70 µmd50
 35 - 105 µmd10-d90
Melt Flow 12 - 18 g/10 min
@Load 2.16 kg,
Temperature 195 °C
180s
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7.00 MPaY; ASTM D638
 40.0 MPaX; ASTM D638
Elongation at Break 800 %X; ASTM D638
 800 %Y; ASTM D638
Elongation at Yield 800 %X; ASTM D638
 800 %Y; ASTM D638
Tensile Modulus 40.0 MPaX; ASTM D638
 40.0 MPaY; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °CASTM D3418
 
Descriptive Properties
ColorOff-WhiteSintered
 White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALP9000 / 312335

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.