FM 958 is a halogen free bedding compound for cable and wire with maximum 90ºC operating temperature at conductor and Insulation: YI 1 - YI 5 PVC (acc. DIN/VDE 0207 Part 4); and Sheathing: YM 1 - YM 5 PVC (acc. DIN/VDE 0207 Part 5); and other standards. Non-flame retardant; PVC Insulation: PVC Sheathing Applications: Market: PolyOne First ChoiceInformation provided by PolyOne Corporation. |