MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 118 MPa
@Temperature 120 °C
Tensile Modulus 7335 MPa
@Temperature 120 °C
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
 35.0 kJ/m²
@Temperature 23.0 °C
Conditioned: 15 days, 70°C, 70% humidity
 37.0 kJ/m²
@Temperature 23.0 °C
Dart Drop, Total Energy 4.50 J
@Temperature -30.0 °C
 9.00 J
@Temperature 23.0 °C
Tensile Creep Modulus, 1000 hours 40.0 MPa
@Temperature 120 °C
 
Descriptive Properties
Commercial StatusEurope
Continuous Vibration Test Cycles70 MpaR= -1
Creep Elongation40%1 hr @ 40 Mpa, 120°C,
 43%1 hr @ 40 Mpa, 150°C,
 50%100 hr @ 40 Mpa, 120°C,
 50%100 hr @ 40 Mpa, 150°C,
 54%1000 hr @ 40 Mpa, 120°C,
 55%1000 hr @ 40 Mpa, 150°C,

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry)
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Conditioned)
BASF Gusspolyamid® Nylon 6 (Dry As Molded)

PBASG0336 / 131969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.