MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hexcel® HexBond™ EA9392 STRUCTIL Two-Component Epoxy Paste
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Thixotropic two-component epoxy adhesive. Its viscosity allows for it to be used for structural bonding, potting, filling, liquid shim and fairing applications. HexBond™ EA9392 STRUCTIL is the toughened version of HexBond™ EA9394 STRUCTIL.

Features:

  • Room temperature curing (= 18oC/64oF)
  • Excellent mechanical properties at temperatures ranging from -55oC/-67oF to 180oC/356oF
  • Good toughness

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Part B
 1.40 g/cc0.0506 lb/in³Part A
Brookfield Viscosity 200000 - 600000 cP200000 - 600000 cPPart A
 300000 - 700000 cP300000 - 700000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength  10.0 MPa
@Temperature 150 °C
1450 psi
@Temperature 302 °F
Lap Shear; EN 2243-1
 17.0 MPa
@Temperature 121 °C
2470 psi
@Temperature 250 °F
Lap Shear; EN 2243-1
 20.0 MPa
@Temperature 80.0 °C
2900 psi
@Temperature 176 °F
Lap Shear; EN 2243-1
 29.0 MPa
@Temperature 22.8 °C
4210 psi
@Temperature 73.0 °F
Lap Shear; EN 2243-1
Peel Strength 6.00 kN/m34.2 pliBell, 23°C
 
Processing PropertiesMetricEnglishComments
Shelf Life  12.0 Month
@Temperature <=23.0 °C
12.0 Month
@Temperature <=73.4 °F
From date of shipment
 12.0 Month
@Temperature <=23.0 °C
12.0 Month
@Temperature <=73.4 °F
From date of shipment
 
Descriptive Properties
ColorAmberPart B
 GreyMixture
 GreyPart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9295 / 322451

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.