360ST1-UV is specifically designed for overmolding with a variety of nylon and glass-filled nylon. Key Features: Excellent surface appearance and good elasticity Outstanding adhesion to nylon in Overmolding process Easy to process and good UV resistance. Application: Soft Touch Grips, Tools, Sports equipment, Electronics, General Purpose, etc.. RoHS Compliance: RoHS Compliant. Appearance: Natural Color. Forms: PelletsInformation provided by Conventus Polymers |