MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics POLASTRIP® Metal EMI Gasket
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shielding is provided by monel or aluminum knitted wire mesh embedded in silicone. POLASTRIP gasketing with solid silicone weather seal are recommended for sealing under high pressure conditions.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 4030 - 40ASTM D2240
Tensile Strength >= 1.72 MPa>= 250 psiASTM D412
Elongation at Break >= 200 %>= 200 %ASTM D412
Tear Strength >= 7.89 kN/m>= 45.0 pliASTM D624
Compression Set 20 %20 %ASTM D395B
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  >= 46 dB
@Frequency 14000 Hz
>= 46 dB
@Frequency 14000 Hz
 >= 93 dB
@Frequency 1e+9 Hz
>= 93 dB
@Frequency 1e+9 Hz
 >= 102 dB
@Frequency 1.80e+7 Hz
>= 102 dB
@Frequency 1.80e+7 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °FSilicone Version
Minimum Service Temperature, Air -57.0 °C-70.6 °FSilicone Version
 
Descriptive Properties
ColorGray
Maximum Joint Unevenness, % of Gasket Height0.17Class B- Open-Close in Same Position
 0.17Class C- Completely Interchangeable
 0.2Class A- Permanently Closed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon CP-301C Bulk Compound
Precision Polymer Engineering E50E Ethylene Propylene Rubber
Overview of materials for Silicone, Molded, Glass Fiber Filled
ATG s.r.l. VMQ Silicone Rubber

PCHOME271 / 130981

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.