MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Belsil® TMS 803 Trimethylsiloxysilicate
Categories: Polymer

Material Notes: BELSIL® TMS 803 is the co-hydrolysis product of tetraalkoxysilane (Q unit) and trimethylethoxysilane (M unit). The chemical structure of BELSIL® TMS 803 can be seen as a three-dimensional network of polysilic acid units, which are endblocked with trimethylsilyl groups. Some residual ethoxy and hydroxy functions are present. BELSIL® TMS 803 is a white powder manufactured in such a way that it is substantially free of aromatic solvents such as toluene. In keeping with its low content of fine dust particles and its uniform particles, BELSIL® TMS 803 exhibits excellent rheological properties (flowability). BELSIL® TMS 803 can be compounded with polydimethylsiloxanes.

Application: This highly cross-linked silicone resin is primarily used for its film-forming attributes. In sunscreen, skincare and color cosmetic applications, the Trimethylsiloxysilicate BELSIL® TMS 803 is an excellent water-resistant additive and helps to hold pigments in place. It prevents agglomeration and maintains free-flowing characteristics in loose powder products. In haircare compositions, the silicone resin provides volume and body, while imparting humidity resistance to the hair.

INCI name: Trimethylsiloxysilicate

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.250 g/ccDIN EN ISO 60
Particle Size 10 µmD50
 
Descriptive Properties
SolubilityBELSIL® DM 0.65>10%
 BELSIL® DM 1 Plus>10%
 BELSIL® DM 10>10%
 BELSIL® DM 1000>10%
 BELSIL® PDM 1000>10%
 BELSIL® PDM 20>10%
 C12-15 alkyl benzoatesinsoluble
 C9-13 isoparaffininsoluble
 Castor oilinsoluble
 Cyclopentasiloxane>10%
 Decyl oleateinsoluble
 Dicaprylyl ether>10%
 Ethanol>10%
 Ethyl acetate>10%
 Ethylhexyl Salicylate1-10%
 Ethylhexyl stearate1-10%
 Glycerolinsoluble
 Hydrogenated Polydeceneinsoluble
 Isododecan>10%
 Isopropanol>10%
 Isopropyl myristate>10%
 Lanolin oilinsoluble
 Myristyl lactate, myristyl alcoholinsoluble
 Oleyl alcoholinsoluble
 Oleyl dodecanolinsoluble
 Oleyl oleateinsoluble
 Olive oilinsoluble
 PEG-7 Glyceryl Cocoateinsoluble
 PEG-75 Lanolin oilinsoluble
 PPG-5-Laureth-5insoluble
 Propylene glycolinsoluble
 Waterinsoluble
 Wheat germ oilinsoluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ALKAMULS® CRH 40 C Surfactant
Solvay ALKAMULS® 14/R Surfactant
Ipiranga Petrochem LBH 0120 BPS LLDP

PWACK9044 / 204573

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.