MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound D551RC Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP D551RC compound is based on recycled Polycarbonate (PC) resin containing 50% glass fiber. Added features of this grade include: High Modulus, Low Warpage, Good Ductility, Non-Brominated & Non-Chlorinated Flame Retardant. Post-Consumer Recycling (PCR) Polycarbonate content up to 30%.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Enhanced Ductility,Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.618 g/cc0.05845 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity  20 cP
@Load 2.16 kg,
Temperature 300 °C
20 cP
@Load 4.76 lb,
Temperature 572 °F
MVR cc/10 min; ASTM D1238
 34.98 cP
@Load 5.00 kg,
Temperature 300 °C
34.98 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 147 MPa21300 psi5 mm/min; ISO 527
Elongation at Break 1.35 %1.35 %5 mm/min; ISO 527
 2.0 %2.0 %5 mm/min; ASTM D638
Tensile Modulus 15.27 GPa2215 ksi1 mm/min; ISO 527
 16.09 GPa2334 ksi5 mm/min; ASTM D638
Flexural Modulus 13.42 GPa1946 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 119 J87.8 ft-lbASTM D256
Izod Impact, Unnotched 4.23 J/cm7.92 ft-lb/inASTM D4812
Charpy Impact Unnotched 3.10 J/cm²14.8 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 13.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
7.28 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 42.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
23.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 3.20 mm
221 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness >=1.00 mm
V-0
@Thickness >=0.0394 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 285 - 305 °C545 - 581 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 285 - 310 °C545 - 590 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa14.5 - 43.5 psi
Screw Speed 50 - 90 rpm50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81492 / 289439

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.