MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® 823 is a two side, differentially pretreated, polyester film designed to provide excellent adhesion in print and lamination applications.

Approvals: FDA Food Contact Status - All gauges of Mylar® 823 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, Sections (f) and (g). This regulation describes films which may be safely used in contact with all types of food, excluding alcoholic beverages, at temperatures not to exceed 250°F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Thickness 0.480 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882A
Film Elongation at Break, TD 70 %ASTM D882A
Coefficient of Friction, Dynamic 0.40ASTM D1894
Coefficient of Friction, Static 0.50ASTM D1894
Film Tensile Strength at Break, MD 31000 psiASTM D882A
Film Tensile Strength at Break, TD 35000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Maximum Service Temperature, Air 250 °F
Shrinkage, MD 1.25 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.50 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64 - 1.67typical of Mylar®
Haze 3.5 %ASTM D1003
Transmission, Visible 90 %TLT; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)6 cc/100 in2O2, 24 hr; ASTM D1434 (77°F/75% RH/1 ATM)
Yield (nominal)42000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 814 Polyester Film, 48 Gauge
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge

PDTZ9266 / 139588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.