MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
Linear Mold Shrinkage, Flow <= 0.00010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 103 MPaASTM D638
Elongation at Break 1.0 %ASTM D638
Tensile Modulus 15200 MPaASTM D638
Flexural Strength 138 MPaASTM D790
Flexural Modulus 12400 MPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cmASTM D257
Surface Resistance <= 1000 ohmASTM D257
 
Processing PropertiesOriginal ValueComments
Melt Temperature 316 - 343 °C
Mold Temperature 135 - 149 °C
Drying Temperature 135 - 149 °C
 
Descriptive Properties
FeaturesElectrically Conductive
 Electromagnetic Shielding (EMI)
 Radio Frequency Shielding (RFI)
FormsPellets
Generic MaterialLCP
Generic NameLiquid Crystal Polymer (LCP)
Processing MethodInjection Molding
Regional AvailabilityNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese CoolPoly® E2 Thermally Conductive Liquid Crystalline Polymer
RTP Company RTP 3499-3 X 92886 Liquid Crystal Polymer (LCP), Thermally Conductive - Electrically Conductive - Sloughing
RTP Company RTP 3499-3 X 117895 F Liquid Crystal Polymer (LCP), Carbon Nanotube - Electrically Conductive
RTP Company RTP 2299 X 115090 B Polyetheretherketone (PEEK), Carbon Nanotube - Electrically Conductive

PH0POL1025 / 145594

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.