MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional LLDPE with the same melt index and shows very good bubble stability. Films obtained with this product have very low gel content. It contains medium antiblocking, medium slip, and medium processing aid additives. Its applications include: automatic packaging (FFS), high performance structures (coextrusion), and frozen bags.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM-D792
Melt Flow 0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 890 %ASTM-D882
Film Elongation at Break, TD 1110 %ASTM-D882
Elmendorf Tear Strength MD 270 gASTM-D1922
Elmendorf Tear Strength TD 590 gASTM-D1922
Elmendorf Tear Strength, MD 7.11 g/micronASTM-D1922
Elmendorf Tear Strength, TD 15.53 g/micronASTM-D1922
Dart Drop 30.26 g/micronASTM-D1709
Dart Drop Test 1150 gASTM-D1709
Film Tensile Strength at Break, MD 50.0 MPaASTM-D882
Film Tensile Strength at Break, TD 40.0 MPaASTM-D882
1% Secant Modulus, MD 270 MPaASTM-D882
1% Secant Modulus, TD 310 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM-D1003
Gloss 75 %Angle 60°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.180 - 0.250 cm
@Temperature 200 - 220 °C
Blown Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.5Blown Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)220max, Blown Film Extrusion
Screen Package40/60/40mesh
Temperature Profile (°C)190-220Blown Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization
CIMBAR RP 9310 Talc
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
AISI 4140 Steel, oil quenched, 425°C (800°F) temper, 25 mm (1 in.) round
AISI 4140 Steel, oil quenched, 315°C (600°F) temper, 25 mm (1 in.) round

PBRAS858 / 106704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.