MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omnia Plastica PA 11 Rilsan B
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: The only engineering plastic of natural origin (derived from castor oil), it is a polyamide which, unlike the other nylons, does not absorb humidity. It has all the good mechanical features of polyamides: tensile stress, compressive strength, wear resistance, etc. Moisture content does not influence its shock resistance. It has very good ageing and low temperature resistance.

Features:

  • Tensile stress, compressive strength and shock resistance values stable in moist as well as dry environments Wear resistance: very good even in dusty or demanding environments.
  • Ageing and low temperature resistance Self-lubricating; low friction coefficient.
  • Generally for sliding applications it does not require lubricators.
  • Colour: natural.
Weak Point:

Although Nylon 11 has all the excellent mechanical features of polyamides without their weakest point (hygroscopicity), its high price prevents wider usage.

Application:

  • Mechanical: thanks to the stability of its excellent mechanical features, both in moist environments and at low temperatures, it is used especially in aeronautic, marine, and transport applications, and in machinery as bushings, bearings, slide and mechanical parts.
  • Food contact: it is physiologically inert and it is used in food processing machinery.
  • Electrical: as it is not hygroscopic and its electrical properties are stable, it is widely used for electrical applications such as insulators.
  • Chemical: it is resistant to solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.90 %50% relative humidity
Water Absorption at Saturation 2.0 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83dry sample; ISO2039.2
Ball Indentation Hardness 100 MPaISO2039.1 DIN.53456
Tensile Strength at Break 45.0 MPaISO.527 DIN.53455
Elongation at Break 270 %ISO.527 DIN.53455
Tensile Modulus 1.80 GPaISO.527 DIN.53455
Compressive Strength 4.00 MPa1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 2.00 J/cm²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.36on dry ground steel; load =0.05MPa; speed =0.6 m/s
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmISO.93 DIN.53482
Dielectric Constant 4.0
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 40.0 kV/mmISO.243 DIN.53481
Dissipation Factor 0.050
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.230 W/m-KDIN.52612
Melting Point 183 °C
Maximum Service Temperature, Air 85.0 °CContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 120 °Cshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO.75 DIN.53461
Minimum Service Temperature, Air -50.0 °Cimpact conditions and heavy loads not considered
Flammability, UL94 V-2
Oxygen Index 22 %ISO.4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Isoflon PA 11 Polyamide 11
Hippe PA 11 Nylon 11
Lucky IF-850 Acrylic, Injection Grade
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled

POMNIA27 / 55618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.