MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® A3Z HP UV BK23220 PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 offers a unique combination of impact performance and excellent processability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi50mm/min; ISO 527
Elongation at Break 50 %50 %50mm/min, Nominal strain; ISO 527
Flexural Modulus 1.703 GPa247.0 ksiISO Data
Izod Impact, Notched (ISO) 83.0 kJ/m²39.5 ft-lb/in²ISO Test
 22.0 kJ/m²
@Temperature -40.0 °C
10.5 ft-lb/in²
@Temperature -40.0 °F
ISO Test
 
Thermal PropertiesMetricEnglishComments
Melting Point 258 °C496 °F10 K/min
 258 °C496 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FISO 75
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3Z HP PA66 (Dry)
Celanese Zytel® 103HSL NC010 PA66
BASF Ultramid® A3Z HP UV PA66 (Dry)
BASF Ultramid® A3Z HP BK20465 PA66 (Dry)
Celanese Zytel® MT409AHS BK010 PA66-I

PBASF9281 / 85045

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.