MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications:Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, ionomers, and ethylene copolymers.

Bynel® Series 4100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • blow molding melt and solid phase thermoforming
  • sheet and tubing
  • Bynel® 41E623 provides outstanding adhesion to EVOH and polyamide.

    Information provided by DuPont™

    This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.900 g/cc0.0325 lb/in³ASTM D792
    Melt Flow 1.7 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    1.7 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 100 °C212 °FFreezing Point, DSC; ASTM D3418
     119 °C246 °FDSC; ASTM D3418
    Vicat Softening Point 71.0 °C160 °FASTM D1525
     
    Processing PropertiesMetricEnglishComments
    Rear Barrel Temperature 120 °C248 °FFor high temperature coextrusions.
     120 °C248 °FFor coextrusion with EVA or EVOH.
    Middle Barrel Temperature 220 °C428 °FFor coextrusion with EVA or EVOH.
     235 °C455 °FFor high temperature coextrusions.
    Front Barrel Temperature 235 °C455 °FFor coextrusion with EVA or EVOH.
     250 °C482 °FFor high temperature coextrusions.
    Adapter Temperature 235 °C455 °FFor coextrusion with EVA or EVOH.
     250 °C482 °FFor high temperature coextrusions.
    Die Temperature 235 °C455 °FFor coextrusion with EVA or EVOH.
     250 °C482 °FFor high temperature coextrusions.

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ExxonMobil Escorene® LD 721.IK Film Resin
    ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
    ExxonMobil Escorene® LD 701.ID Blown Film Resin
    DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness
    DuPont™ Nomex® 430 1200 Denier Aramid Yarn

    PDUP909 / 33476

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.