MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds Ecoflex™ GEL 2 Platinum Cure Silicone Rubber Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Ecoflex™ GEL 2 is an extremely soft, platinum silicone rubber gel specifically designed for creating medical simulation devices, silicone makeup appliances, for cushioning, creating gaskets, encapsulation, outside-the-body shaping and enhancement products, silicone babies, theatrical prosthetics and more. and other applications requiring a very soft silicone material. Ecoflex™ GEL 2 has a Shore hardness of 000-34, this is below the Shore 00 hardness scale. An infinite number of color effects can be achieved by adding Silc Pig™ silicone pigments. Certified Skin Safe - Cured material is skin safe and certified by an independent laboratory. Ecoflex™ GEL 2 is mixed 1A:1B by weight or volume. Rubber cures at room temperature (73°F / 23°C) with negligible shrinkage. Differences between cured Ecoflex™ Gel 2 and original Ecoflex™ Gel include; Gel 2 is “dryer” and slightly less sticky. While the Shore hardness is about the same, the Gel 2 has a higher modulus that makes this gel feel firmer. Like the original, Gel 2 cannot be handled as a “stand alone” product. It should be encapsulated in another silicone like Dragon Skin, Q-Ballz encapsulant or other suitable membrane.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D-1475
Viscosity 5000 cP5000 cPASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 3434000; ASTM D-2240
Elongation at Break >= 1000 %>= 1000 %ASTM D-412
 
Processing PropertiesMetricEnglishComments
Cure Time 50.0 min0.833 hour
Pot Life 20.0 min20.0 minASTM D-2471
 
Descriptive Properties
ColorTranslucent
Mix Ratio1A:1Bby volume or weight
Specific Volume26.4[in3/lb], ASTM D-1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN333 / 297034

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.