Notes: Monprene CP-10140H, available in NAT and colors, is a high performance thermoplastic elastomer designed for consumer product applications requiring a soft, rubber-like feel. Monprene CP-10140H is a low density, low hardness, halogen free grade that is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Chemical Resistant; Good Colorability; Good Flexibility; Good Moldability; Good Toughness; Halogen Free; High Flow; Low Density; Low Hardness; Low Specific Gravity; Resilient; Slip; Without Fillers Uses: Bladders; Bushings; Connectors; Consumer Applications; Flexible Grips; Grommets; Handles; Knobs; Plugs; Prototyping; Rubber Replacement; Safety Equipment; Seals RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |