MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Pebax® 4033 SP 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccISO 1183
 1.00 g/ccCond.; ISO 1183
 0.830 g/cc
@Temperature 220 °C
Melt
Water Absorption 1.2 %Dry; Sim. to ISO 62
Moisture Absorption 0.500 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmDry; ISO 294-4, 2577
 0.011 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 3.00 sec
Dry; ISO 7619-1
Hardness, Shore D 35
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength at Break 40.0 MPaDry; ISO 527-1/-2
Tensile Stress at Strain 5.00 MPa
@Strain 10 %
Dry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 >= 50 %Cond.; ISO 527-1/-2
 >= 300 %Dry; ISO 527-1/-2
Tensile Modulus 71.0 MPaCond.; ISO 527-1/-2
 73.0 MPaDry; ISO 527-1/-2
50% Modulus 9.00 MPa
@Strain 50 %
Dry; ISO 527-1/-2
 9.00 MPa
@Strain 50 %
Cond.; ISO 527-1/-2
100% Modulus 11.0 MPa
@Strain 100 %
Dry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Tear Strength 85.0 kN/mDry; ISO 34-1
Abrasion 48mm³; Dry; ISO 4649
Compression Set 32 %
@Temperature 23.0 °C,
Time 86400 sec
Dry; ISO 815
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.60e+13 ohm-cmDry; IEC 60093
Surface Resistance 3.00e+12 ohmCond.; IEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 7.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 39.0 kV/mmDry; IEC 60243-1
Dissipation Factor 0.0604
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.071
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 195 µm/m-°CDry; ISO 11359-1/-2
Specific Heat Capacity 2.80 J/g-°CMelt
Thermal Conductivity 0.180 W/m-K
@Temperature 220 °C
Melt
Melting Point 160 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °CDry; ISO 75-1/-2
Vicat Softening Point 131 °C50°C/h 50N; Dry; ISO 306
Glass Transition Temp, Tg -65.0 °C10°C/min; Dry; ISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °CInjection Molding; ISO 294
Mold Temperature 30.0 °CInjection Molding; ISO 10724
Injection Velocity 200 mm/secInjection Molding; ISO 294
Hold Pressure 30.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 7033 SP 01 Polyether Block Amide (PEBA)

PARKG714 / 142509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.