MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Information from Shinkong Synthetic Fibers Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.14 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 550 kg(f)/cm²ASTM D638
Elongation at Break 10 %ASTM D638
Flexural Yield Strength 770 kg(f)/cm²ASTM D790
Flexural Modulus 20500 kg(f)/cm²ASTM D790
Izod Impact, Notched 75.0 kg-cm/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 80.0 kg-cm/cm
@Thickness 3.17 mm,
Temperature -20.0 °C
ASTM D256
 90.0 kg-cm/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Techmer ES Plastiblend® PC/PBT IM 1799 BK
MRC Polymers NAXALOY™ 780 PC+PBT Polyester Blend
Omni Plastics OmniCarb™ PC/PBT 1320 CTI PC/PBT

PSHNK024 / 120794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.