MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ALM Ultrasint® PA6 LM Nylon 6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Ultrasint PA6 LM is a special powder material designed to maximize production accessibility to any PBF user.

Highlights:

  • Low melting Polyamide 6-based powder for Laser Sintering
Applications:
  • Functional prototypes (i.e. in automotive industries)
  • High performance spare parts
  • Multi-purpose industrial goods
  • Durable and rigid jigs & fixtures

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 g/ccDIN EN ISO 60
Density 1.37 g/ccPrinted Part; DIN EN ISO 1181-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 18.0 MPa
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 25.0 MPa
@Temperature 80.0 °C
X-Direction; ISO 527-2
 28.0 MPa
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 38.0 MPa
@Temperature 23.0 °C
X-Direction; ISO 527-2
Elongation at Break 5.5 %
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 7.8 %
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 17 %
@Temperature 23.0 °C
X-Direction; ISO 527-2
 24 %
@Temperature 80.0 °C
X-Direction; ISO 527-2
Tensile Modulus 600 MPa
@Temperature 80.0 °C
Z-Direction; ISO 527-2
 650 MPa
@Temperature 80.0 °C
X-Direction; ISO 527-2
 1350 MPa
@Temperature 23.0 °C
Z-Direction; ISO 527-2
 1500 MPa
@Temperature 23.0 °C
X-Direction; ISO 527-2
Flexural Modulus 1200 MPaZ-Direction; DIN EN ISO 178
 1450 MPaX-Direction; DIN EN ISO 178
Izod Impact, Notched (ISO) 5.30 kJ/m²Z-Direction; ISO 180
 6.60 kJ/m²X-Direction; ISO 180
Izod Impact, Unnotched (ISO) 6.00 kJ/m²Z-Direction; ISO 180
 28.0 kJ/m²X-Direction; ISO 180
Charpy Impact Unnotched 9.70 kJ/m²Z-Direction; ISO 179-1
 52.0 kJ/m²X-Direction; ISO 179-1
Charpy Impact, Notched 4.20 kJ/m²Z-Direction; ISO 179-1
 5.60 kJ/m²X-Direction; ISO 179-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALP9024 / 312359

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.