MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Inhibitors 200
Categories: Polymer; Thermoplastic; Silicone, Thermoplastic

Material Notes: Inhibitors are used for setting the pot life of platinum-catalyzed, addition-cured silicones.

Application: Inhibitors MVC and DVS are pure silicone-based inhibitors which control the activity of the Pt-catalyst. They are used when exceptionally long working times or very low dosage levels are required. The typical dosage is between 0.01 and 1 %. Inhibitors 200 – 600 are ready-to-use mixtures of various alkinol or silicone based inhibitors in Polymer VS. Depending on the required pot life, the dosage is typically between 1 and 10 %. The below diagram shows the effect of the various inhibitor solutions in a two component addition-cure silicone formulation. It shows the required inhibitor concentration to get a working time of 40 minutes. Another important parameter is the volatility of the inhibitor. A high volatility is preferred e. g. in heat cure coatings. Here, a fast evaporation leads to a quick full cure at the moment of heating. However, in such formulations working time can shorten during open storage of the components. Low volatile inhibitors are typically used when vulcanization shrinkage and VOC are to be minimized.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 500 cP
 
Descriptive Properties
AppearanceClear, colorless liquid
Content1.2 mmol/gVinyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Inhibitors MVC
Overview of materials for Precipitation Hardening Stainless
Overview of materials for T S10000 Series Stainless Steel
Multibase TPSiV® 3011-50A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3010-50A Thermoplastic Silicone Vulcanizate

PEVONIL976 / 197180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.