MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® LT-302 Fluoroelastomer Terpolymer, 64% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® LT-302 is a terpolymer suitable for various peroxide cure systems. LT-302 can be formulated to eliminate the post cure process. LT-302 is designed for transfer and compression molding applications that require a balance between good low temperature flexibility and compression set resistance.

Typical Applications: O-Rings, gaskets, molded tubing

Rheological Properties:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.79 g/cc1.79 g/cc
Mooney Viscosity 44
@Temperature 121 °C
44
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868
Tensile Strength at Break 20.5 MPa2970 psi
 22.1 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
3210 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
Elongation at Break 250 %250 %
 275 %
@Treatment Temp. 200 °C,
Time 252000 sec
275 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
100% Modulus 4.40 MPa
@Strain 100 %
638 psi
@Strain 100 %
Compression Set  10 %
@Temperature 175 °C,
Time 252000 sec
10 %
@Temperature 347 °F,
Time 70.0 hour
#214 O-ring; ASTM D395 Method B
 19 %
@Temperature 200 °C,
Time 252000 sec
19 %
@Temperature 392 °F,
Time 70.0 hour
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -30.0 °C-22.0 °FLow Temperature Retraction, TR10
 
Processing PropertiesMetricEnglishComments
Cure Time 0.400 min0.00667 hourts2, scorch time, MDR 2000
 0.500 min0.00833 hourt'50, time to 50% cure, MDR 2000
 0.700 min0.0117 hourt'90, time to 90% cure, MDR 2000
 10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
Press Cure
 240 min
@Temperature 200 °C
4.00 hour
@Temperature 392 °F
Post cure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 64 %64 %
 
Descriptive Properties
ColorWhite to light pink
MH26 dNmmaximum torque, MDR 2000
ML1.1 dNmminimum torque, MDR 2000
Test Formula100 phrDAI-EL® LT-302
 3 phrPeroxide (50% Activity)
 3 phrZinc Oxide
 30 phrMT Carbon Black (N-990)
 4 phrTAIC (72% Activity)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9864 / 209935

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.