MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccASTM D792
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 6.0 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 96.0 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.86 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 2.13 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CASTM D648
UL RTI, Electrical 75.0 °C
UL RTI, Mechanical with Impact 75.0 °C
UL RTI, Mechanical without Impact 75.0 °C
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 495 - 535 °F
Middle Barrel Temperature 475 - 535 °F
Front Barrel Temperature 475 - 535 °F
Nozzle Temperature 475 - 535 °F
Melt Temperature 475 - 535 °F
Mold Temperature 160 - 200 °F
Drying Temperature 190 - 210 °F12 hours maximum
 210 °F4 hours minimum
Dew Point -40.0 °CPreferred
 <= -20.0 °C
Injection Pressure 16000 - 20000 psi
Back Pressure 100 - 200 psi
Shot Size 50 - 70 %
Vent Depth 0.000800 - 0.00100 in
Screw Speed 40 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS PCA-3013 High Flow PC/PBT Alloy
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled
PTS PBT-15GF 15% Glass Filled PBT

PZ9PU43g / 21581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.