MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Polygon Composites PolyMed® CW Circumferential Fiber Engineered Composite Orientation Medical Tubing
Categories: Polymer; Thermoset

Material Notes: PolyMed® Circumferentially Fiber Orientation tubing utilizes multidirectional fibers oriented both helically and axially, with thermoset resin as the matrix. Our most popular product for medical device applications, PolyMed CW tubing provides a high strength tube with excellent elasticity.

Key Features:

  • High strength-to-weight ratio
  • Improved hoop strength
  • Outstanding dielectric properties
  • Electromagnetically transparent
  • Proven bio-compatibility
  • USP Class VI and ISO10993 compliant
  • Non-reflective characteristics
  • Compatible with conventional sterilization processes

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 %as produced
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.0 ksiASTM D638
Tensile Modulus 5000 ksiASTM D638
Flexural Strength 60.0 ksiASTM D790
Flexural Modulus 4000 ksiASTM D790
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/mil
 150 V/mil
@Time 57600 sec
after water soak and 20 autoclave cycles
 250 V/mil
@Time 57600 sec
after water soak
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Basotect G Foam
Asahi Kasei Xyron™ A0210 PA/PPE
Asahi Kasei Thermylon® N3-30FG-1626 PA66-GF30
Asahi Kasei Leona™ 91G40 Polyamide 66, MF Reinforced
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy

PPOLYG02 / 184502

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.