MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Network Polymers Softflex® 3300
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.868 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0392 cm/cm
@Thickness 3.17 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0392 cm/cm
@Thickness 3.17 mm
ASTM D955
Melt Flow 3.4 g/10 min
@Load 1.00 kg,
Temperature 235 °C
Procedure A Condition Q; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26 - 3610 second dwell; ASTM D2240
 37 - 47Instantaneous; ASTM D2240
Tensile Strength at Break 373 psichs 20 in/min; ASTM D412
Elongation at Break >= 1000 %ASTM D412
50% Modulus 0.000560 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.000700 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.000960 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 585 psiTest Method I (chs speed 0.5 in/min)
Tear Strength 12.4 kN/mDie C/20"/min; ASTM D624
Taber Abrasion, mg/1000 Cycles 0.0013H22 Wheel 1000 g load/1000 cycles; ASTM D3389
Compression Set 61.4 %
@Temperature 100 °C
22 hours at 25% deflection; ASTM D395, Method B,
 72.6 %
@Temperature 70.0 °C
22 hours at 25% deflection; ASTM D395, Method B,
 25.9 %
@Temperature 23.0 °C,
Time 79200 sec
Method B, at 25% deflection; ASTM D395
Tensile Set 8.6 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Network Polymers Softflex® 5000
Network Polymers Softflex® 5300
Network Polymers Softflex® 0350
Network Polymers Softflex® 0470
CPT C-Flex® R70-001 Opaque Biocompatible TPE

PDIAM012 / 29850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.