TRA-PAD PCAA8A is a non-silicone, phase change material. It provides low thermal resistance and ease of assembly. It is designed to provide heat dissipation in processors and high power devices. Typical applications include providing maximum heat transfer between an active device and a heat spreader or heat sink. Information provided by Tra-Con Inc. |