MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
712-8 Nextrema® Opaque Grey Glass Ceramic/SCHOTT
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:
  • Very low coefficient of linear thermal expansion
  • Excellent temperature and thermal shock resistance
  • High transmission in infrared range and unique visible light transmission profiles with different specific grades
  • Excellent chemical resistance
High mechanical strength technical data presented herein are typical averages.

Vendors: NEXTREMA® glass-ceramics from SCHOTT combines the benefits of technical glasses with properties of high temperature materials.
General Brochure
Visit our web site and view the NEXTREMA® movies.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.52 g/cc
Porosity 0.00 %ISO 9385
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 2.0DIN 12116
Alkali Class, AR 2.0ISO 695
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 600HK 0.1 / 20; ISO 9385
Modulus of Elasticity 84.0 GPaASTM C-1259
Flexural Strength 125 MPaBending sbB; DIN EN 1288, Part 5, R45
Poissons Ratio 0.26ASTM C-1259
Shear Modulus 33.3 GPaCalculated by MatWeb
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 400000 ohm-cm
@Temperature 350 °C
DIN 52326
 1.30e+7 ohm-cm
@Temperature 250 °C
DIN 52326
Dielectric Constant 7.3
@Frequency 1e+6 Hz,
Temperature 25.0 °C
DIN 53483
Dielectric Loss Index 0.0040
@Frequency 1e+6 Hz,
Temperature 25.0 °C
DIN 53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.840 µm/m-°C
@Temperature 20.0 - 300 °C
 1.60 µm/m-°C
@Temperature 300 - 700 °C
Specific Heat Capacity 0.830 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 1.50 W/m-K
@Temperature 90.0 °C
DIN 51936, ASTM E 1461-01
Maximum Service Temperature, Air 470 °C
@Time 1.80e+7 sec
Inhomogeneous Heating
 520 °C
@Time 3600 sec
Inhomogeneous Heating
 850 °C
@Time 1.80e+7 sec
Homogeneous Heating
 950 °C
@Time 3600 sec
Homogeneous Heating
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %
@Thickness 4.00 mm,
Wavelength 600 nm
 0.00 %
@Thickness 4.00 mm,
Wavelength 700 nm
IR Transmittance 2.0 %
@Thickness 4.00 mm,
Wavelength 1000 nm
 25 %
@Thickness 4.00 mm,
Wavelength 1600 nm
 70 %
@Thickness 4.00 mm,
Wavelength 2500 nm
UV Transmittance 0.00 %
@Thickness 4.00 mm
 
Descriptive Properties
Acoustical Characteristic, vlong.6520 m/s
AppearanceOpaque
ColorGrey
Hydrolytic Resistance HGB1DIN ISO 719
tk100(°C)202specific electric volume resistivity of 108 O·cm
Thermal Shock Resistance (TSR)700°CResists cold water without cracking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
712-3 Nextrema® Tinted Glass Ceramic/SCHOTT
724-8 Nextrema® Opaque White Glass Ceramic/SCHOTT
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic
Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition
724-5 Nextrema® Translucent White Glass Ceramic/SCHOTT

CSGS802 / 178426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.