MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen EP440M Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP440M is a high isotacticity polypropylene impact copolymer with an optimized balance of stiffness and toughness, high impact strength at low temperature, high stiffness and low warpage. Typical customer application is injection molding of battery cases. Applications: Battery Cases

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97ASTM D785
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 1200 MPaASTM D790
Izod Impact, Notched 40.0 J/m
@Temperature -20.0 °C
ASTM D256
 100 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
Vicat Softening Point 150 °CASTM D1525
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen EP440M Injection Molding Grade Polypropylene
Bamberger Polymers Bapolene® 5010NB Polypropylene, Extrusion Grade
M. Holland Company CP300 Polypropylene Copolymer
Aurora Plastics TufGuard M™ GPP1005M-EXLT PP, Flame Retardant
Aurora Plastics TufGuard M™ GPP1005M-CD PP, Flame Retardant

PEQT8939 / 220573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.