MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cariflex IR0401 BU Polyisoprene Rubber Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Cariflex™ IR0401 BU Latex is a water-based emulsion of an anionically polymerized polyisoprene with a high cis-1,4 content, high molecular weight and a high linearity. The emulsion also contains a non-staining antioxidant (typical level of 0.1% mass on solids) and a surfactant.

Uses: Cariflex™ IR0401 BU Latex is a synthetic rubber emulsion and can be used as an alternative to natural rubber latex in a variety of applications ranging from dipping to extrusion. It offers specific advantages such as light color, consistency and low levels of impurities. Cariflex™ IR0401 BU Latex is made under Good Manufacturing Practices, but additional requirements may apply to food contact, pharmaceutical and medical device applications using this material.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Medical; and Personal Care

Information provided by Kraton®. Kraton sold the Cariflex product line to Daelim Industrial in 2020.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccISO 2781
Solids Content >= 63 %KM 42
Particle Size <= 1.8 µmMedian; KM 45
pH 9.5 - 12KM 43
Brookfield Viscosity <= 150 cPKM 44
Molecular Weight 1.50e+6 - 2.50e+6 g/molKM 49
Ash <= 0.10 %KM 35
 
Thermal PropertiesOriginal ValueComments
Melting Point 0.000 °CFreezing
 
Descriptive Properties
AppearanceMilky White
Content1,4-Cis, FTIR>90%, KM34
 1,4-Cis, NMR>82%, KM34
 Antioxidant0.15, KM31
 Gel content0 percent
 LIV6.0-7.6 dL/g, KM 33
 LVN6.7-9.2 dL/g, KM 33
OdorNeutral
T.A.M.C. at drumming<1000 CFU/mlUSP24 (61)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cariflex IR0401 SU Polyisoprene Rubber Latex
Cariflex IR0310 K Polyisoprene
Cariflex IR0307 K Polyisoprene
AlphaGary Evoprene™ HP 3704 High Performance Thermoplastic Elastomer
Kraton® FG1901 + PA-6 blend (20/80)

PKRA9925 / 132825

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.